BUTADIENE RUBBERS (BR)

The BR family of polybutadiene rubber helps optimize tire compositions, improving grip, fuel economy, and overall lifetime. They provide a great balance between processability and performance.

Buna® Nd 24 EZ Easy Processing Nd-BR (Buna Nd)
Property Nominal Value Test Method Condition Temperature
Mooney Viscosity 44 MU ISO 289 / ASTM D 1646 ML (1+4) 100 °C
Cis 1,4 Content > 96 %
Density 0,91 g/cm3 ASTM D 297

Chloroprene Rubber

Chloroprene rubber (international ASTM/DIN-abbreviation: CR) is a high-performance material with a wide variety of applications. Baypren® is the brand-name of the ARLANXEO range of polymers based on 2-chloro-1,3-butadiene (chloroprene), which are manufactured by water-based emulsion polymerization....

Baypren® 110 M 41 M-modified Grades
Property Nominal Value Test Method Condition Temperature
Mooney Viscosity 41 MU ISO 289 / ASTM D 1646 ML (1+4) 100 °C
Density 1,23 g/cm3 Internal Method
Baypren® 110 M 49 M-modified Grades
Property Nominal Value Test Method Condition Temperature
Mooney Viscosity 49 MU ISO 289 / ASTM D 1646 ML (1+4) 100 °C
Density 1,23 g/cm3 Internal Method

EMULSION-STYRENE BUTADIENE RUBBERS (E-SBR)

E-SBR is predominantly used for the production of car tires, light truck tires and truck tire retread compounds. It presents good mechanical properties, abrasion, and tear resistance.

Buna® SE 1500 Oil-free E-SBR
Property Nominal Value Test Method Condition Temperature
Mooney Viscosity 52 MU ISO 289 / ASTM D 1646 ML (1+4) 100 °C
Bound Styrene 23,5 wt % ASTM D 5775
Density 0,94 g/cm3 ASTM D 297
Buna® SE 1502 H Oil-free E-SBR
Property Nominal Value Test Method Condition Temperature
Mooney Viscosity 53 MU ISO 289 / ASTM D 1646 ML (1+4) 100 °C
Bound Styrene 23,5 wt % ASTM D 5775
Density 0,94 g/cm3 ASTM D 297
Buna® SE 1502 L Oil-free E-SBR
Property Nominal Value Test Method Condition Temperature
Mooney Viscosity 49 MU ISO 289 / ASTM D 1646 ML (1+4) 100 °C
Bound Styrene 23,5 wt % ASTM D 5775
Density 0,94 g/cm3 ASTM D 297

Ethylene Propylene Diene Rubber

EPDM is typically used in outdoor applications and at elevated temperatures of up to 150 °C. It's used in both automotive and industrial applications such as automotive sealing systems, coolant hoses, windshield wipers, oil additives, roof sheeting, window gaskets, conveyor belts, as well as wire...

Keltan® 10660C Very high Mooney
Property Nominal Value Test Method Condition Temperature
Mooney Viscosity 66 MU ISO 289 / ASTM D 1646 ML (1+8) 150 °C
Molecular Weight Distribution CLCB Internal Method
Ethylene Content 56 wt % ASTM D 3900
ENB Content 6,5 wt % ASTM D 6047
Density 0,86 g/cm3 Internal Method
Keltan® 2470C Low Mooney
Property Nominal Value Test Method Condition Temperature
Mooney Viscosity 22 MU ISO 289 / ASTM D 1646 ML (1+4) 125 °C
Molecular Weight Distribution CLCB Internal Method
Ethylene Content 70,5 wt % ASTM D 3900
ENB Content 4,5 wt % ASTM D 6047
Density 0,86 g/cm3
Keltan® 2470S Low Mooney
Property Nominal Value Test Method Condition Temperature
Mooney Viscosity 25 MU ISO 289 / ASTM D 1646 ML (1+4) 125 °C
Molecular Weight Distribution CLCB Internal Method
Ethylene Content 69 wt % ASTM D 3900
ENB Content 4,2 wt % ASTM D 6047
Density 0,86 g/cm3 Internal Method
Keltan® 2650C Low Mooney
Property Nominal Value Test Method Condition Temperature
Mooney Viscosity 25 MU ISO 289 / ASTM D 1646 ML (1+4) 125 °C
Molecular Weight Distribution CLCB Internal Method
Ethylene Content 46 wt % ASTM D 3900
ENB Content 6,0 wt % ASTM D 6047
Density 0,86 g/cm3 Internal Method
Keltan® 3960 Low Mooney
Property Nominal Value Test Method Condition Temperature
Mooney Viscosity 54 MU ISO 289 / ASTM D 1646 ML (1+8) 100 °C
Molecular Weight Distribution Medium Internal Method
Ethylene Content 56 wt % ASTM D 3900
ENB Content 11,0 wt % ASTM D 6047
Density 0,86 g/cm3 Internal Method
Keltan® 4465 Medium Mooney
Property Nominal Value Test Method Condition Temperature
Mooney Viscosity 48 MU ISO 289 / ASTM D 1646 ML (1+4) 125 °C
Molecular Weight Distribution Broad Internal Method
Ethylene Content 56 wt % ASTM D 3900
ENB Content 4,1 wt % ASTM D 6047
Oil Content 50 PHR ISO 1407
Density 0,87 g/cm3 Internal Method
Keltan® 5470
Regional
Medium Mooney
Property Nominal Value Test Method Condition Temperature
Mooney Viscosity 55 MU ISO 289 / ASTM D 1646 ML (1+4) 125 °C
Molecular Weight Distribution CLCB Internal Method
Ethylene Content 70 wt % ASTM D 3900
ENB Content 4,6 wt % ASTM D 6047
Density 0,86 g/cm3 Internal Method
Keltan® 5470C Medium Mooney
Property Nominal Value Test Method Condition Temperature
Mooney Viscosity 55 MU ISO 289 / ASTM D 1646 ML (1+4) 125 °C
Molecular Weight Distribution CLCB Internal Method
Ethylene Content 66 wt % ASTM D 3900
ENB Content 4,6 wt % ASTM D 6047
Density 0,86 g/cm3 Internal Method
Keltan® 6470C High Mooney
Property Nominal Value Test Method Condition Temperature
Mooney Viscosity 63 MU ISO 289 / ASTM D 1646 ML (1+4) 125 °C
Molecular Weight Distribution CLCB Internal Method
Ethylene Content 64 wt % ASTM D 3900
ENB Content 4,8 wt % ASTM D 6047
Density 0,86 g/cm3 Internal Method
Keltan® 6471 High Mooney
Property Nominal Value Test Method Condition Temperature
Mooney Viscosity 65 MU ISO 289 / ASTM D 1646 ML (1+4) 125 °C
Molecular Weight Distribution Narrow Internal Method
Ethylene Content 67,5 wt % ASTM D 3900
ENB Content 4,7 wt % ASTM D 6047
Oil Content 15 PHR ISO 1407
Density 0,86 g/cm3 Internal Method